Safety perfomance
- Tempered glazing
In the event of breakage, the fine fragmentation of tempered glass into many small pieces reduces the risk of injuries.
- Laminated glazing
- 2 per EN 12600 standard :
Types of risks | Hard body drop test per EN 12600 |
injuries | 2B2 |
injuries and falls | 1B1 |
It is essential to comply with the DTU 39 building regulations to ensure that the test performance level is maintained in the built structure.
- 7 per EN 356 standard :
Type of risks |
Steel sphere drop test per EN 356 |
Hammer and axe test per EN 356
|
manual attack (vandalism) | P1A to P5A | |
manual attack and break in | P6B and P7B |
It is essential to comply with the DTU 39 building regulations to ensure that the test performance level is maintained in the built structure.